合金鋼板檢材料的進場驗收,復驗按批進行,標志應粘貼牢固、字跡清晰,包裝材料應符合有關法律規定,每批交貨的鋼板必須有質量保證文件和力學性能試驗報告。
Alloy steel materials approach acceptance, re inspection according to the batch, logo should be pasted firmly, clear handwriting, packaging materials should comply with the relevant laws and regulations, must have quality assurance and mechanical performance test report file delivery of each batch of steel plate.
尤其是汽車用合金鋼板在動態條件下的拉伸性能檢測變得越來越重要。然而,不同檢測實驗室采用的檢測方法不同,沒有可利用的檢驗標準,并且生成的數據通常不具有可比性。為了提高鋼在高速拉伸試驗條件下的數據質量,12Cr1MOV合金鋼板提高碰撞模擬的準確性。
Especially the tensile performance testing of automotive alloy steel plate under dynamic conditions becomes more and more important. However, the detection methods used by different testing laboratories are different, there are no available inspection standards, and the generated data are usually not comparable. In order to improve the data quality of steel under high tensile test conditions, 12Cr1MOV alloy steel plate was used to improve the accuracy of collision simulation.
從適用范圍、設備器材、檢測條件和方法、對比試塊、靈敏度的調校、缺陷的測定與評定等幾方面對國內外常用鋼板超聲檢測標準進行對比分析,為有關單位和檢驗人員更加深入地理解和使用標準,正確執行標準提供參考。
Analyzed from the scope, equipment, test conditions and methods, contrast test block, adjust the sensitivity of defect testing and evaluation of several aspects of commonly used at home and abroad steel plate ultrasonic testing standards for personnel and inspection of the relevant units of more in-depth understanding and use of standard, the correct reference standard.
其中對各等級的文字描述為:
The text of each grade is described as:
A級:全面地覆蓋著氧化皮,允許有微量銹斑(直徑不大于10mm)的鋼材表面;
Class A: fully covered with oxide, allow trace rust (diameter less than 10mm) of the steel surface;
B級:已發生銹蝕并且部分氧化皮已經剝落的鋼材表面,剝落面積不超過總氧化表面積的1/10;
Grade B: steel surface that has corroded and partially oxidized the peel has peeled off the area of not more than the total oxidation surface area of 1/10;
C級:氧化皮已因銹蝕而剝落,或者可以刮除,并且有少量點蝕的鋼材表面;
Grade C: the surface of the oxide has been peeled off due to rust, or can be scraped, and a small amount of pitting steel surface;
D級:氧化皮已因銹蝕而全面剝落,并且已普遍發生點蝕的鋼材表面。n
Grade D: oxide skin has been completely peeled off due to rust, and has generally pitting steel surface. N
相信看了本文的介紹后,對濟鋼代理商的這方面也會有自己的一番認識,以后針對http://www.ctmpfsc.com必須要嚴格等問題也能很好的解決。
Believe that the introduction of this article, will also have a new understanding of the Jinan agents, later for http://www.ctmpfsc.com must be strict and other issues also can be a good solution.